IPE 600 vs IPN 600

Steel section comparison · IPE / IPN · EN 10365

  • IPE 600 is 38 % lighter than IPN 600 (122.4 vs 199.0 kg/m).
  • IPN 600 has 51 % higher strong-axis stiffness Iy.
  • IPN 600 has 38 % higher weak-axis stiffness Iz, which governs columns and lateral stability.
  • IPN 600 has 55 % higher plastic bending resistance (Wpl,y).
  • Per kilogram of steel, IPE 600 is the more efficient bending section (Iy/G: 752 vs 698 cm⁴ per kg/m).
PropertyIPE 600IPN 600
Height h [mm]600600
Flange width b [mm]220215
Web thickness tw [mm]12.021.6
Flange thickness tf [mm]19.032.4
Area A [cm²]156.0253.7
Mass G [kg/m]122.4199.0
Moment of inertia Iy [cm⁴]92 080139 000
Elastic modulus Wel,y [cm³]3 0694 630
Plastic modulus Wpl,y [cm³]3 5125 452
Moment of inertia Iz [cm⁴]3 3874 670
Radius of gyration iy [mm]243.0234.0
Radius of gyration iz [mm]46.643.0
Torsion constant It [cm⁴]164.6787.0
Warping constant Iw [×10³ cm⁶]2 814.73 814.0

Highlighted value = the favourable one (higher stiffness/modulus, lower mass). Full property sets on the profile pages.

Explore further

Disclaimer: All content, data, and calculations on this website are provided "as is" for informational purposes only. While we strive for accuracy, we do not warrant that the content is complete, up-to-date, or free of errors. The content does not constitute professional advice and must be verified against the official applicable standards by a qualified person. Use of this data is strictly at the user's own risk, and we accept no liability for any direct or indirect damages resulting from its use.